HOT METAL LADLE

Working Lining Bottom & Side Wall

BRAND NAME MgO ≥ SiO2 ≤ Al2O3 ≤ Fe2O3 ≤ CaO ≤ Residual Carbon (C) C.C.S. (MPa) ≥ B.D. (g/ cm3) ≥ A.P. (%) ≤ CAP (1100 °C/2 hrs) Max. HMOR (1400 °C/30 min) Min.
HMASC-21F 5.0 72 1.0 4-6 50 3.00 8
HMASC-22FP 8.0 53 1.0 8-10 50 2.65 8
HMASC-22F 8.0 68 1.8 8-10 45 2.90 7
HMASC-22B 7.0 60 1.8 8-10 50 2.80 8
HMAL-80 78 1.8 60 2.75 20
HMAL-80-C 78 1.6 70 2.75 20
HMAL-70FB 65 2.0 60 2.65 20

Free Board

HMAL 60B-C 60 1.8 60 2.50 22
HMAL 50BC 50 2.0 60 2.34 22

Insulation

HMINSBAL-45 43 55 1.0 0.5
HMINSBAL-50 45 55 1.0 0.7

Unshaped (Monolithic)Refactory

BRAND NAME MgO ≥ SiC ≤ Al2O3 ≤ Fe2O3 ≤ CaO ≤ Residual Carbon (C) C.C.S. (MPa) ≥ B.D. (g/ cm3) ≥ A.P. (%) ≤ Grain Size Self Line Months
HML CASTAL-70 65 2.0 60 2.45 0-6 6
HML CASTAL-80 78 1.5 50 2.50 0-6 6
HML CASTAL-90 85 1.5 60 2.65 0-8 6
MORT ASC-70 7.0 60 2.0 0-1 6
MORTAL-50 48 2.0 0-1 6
MORTAL-70 65 2.0 0-1 6
HML CASTAL-50 48 2.0 50 2.2 0-6 6